       半消光長絲尼龍6, is widely used in warp knitting, machine weaving, luggage fabrics, sportswear, underwear, and industrial textiles. Downstream weaving and dyeing factory customers are most concerned about batch stability, breakage rate, and dyeing consistency. A comprehensive factory inspection can reduce complaints such as broken wires, color differences, and inconsistent shrinkage in the subsequent process. Below is a complete introduction to the routine factory inspection items for semi dark filament nylon 6, to assist the purchaser in incoming material acceptance and supplier quality control.

一、物理機械性質檢測(核心必填項目)

1.線密度和線密度變異係數(CV)

       According to the GB/T14343 standard, measure the actual denier/dtex value of the silk, calculate the deviation of linear density and CV value. Large fluctuations in line density can directly cause uneven fabric weight and stripe marks on the fabric surface. The procurement and acceptance of semi dark nylon 6 filament generally agree on the range of linear density deviation, and the lower the CV value, the more uniform the filament.

2.斷裂強度和斷裂伸長率

       According to GB/T14344 testing, it reflects the ability and toughness of the silk thread to withstand tensile force. Insufficient strength can lead to breakage during the weaving process; The elongation rate is unstable, and the stretch rebound of the finished fabric is inconsistent. Sports fabrics, seat belts, luggage fabrics, etc. have higher requirements for strength indicators.

3.沸水收縮率

       GB/T6505 standard testing is a crucial indicator for nylon filament. Nylon 6 will shrink when exposed to hot water, and the shrinkage rate fluctuates greatly in boiling water. After dyeing and shaping, the fabric is prone to uneven length and wrinkles. Customers will specify corresponding shrinkage rate ranges for different application scenarios.

4.帶材均勻度(帶材CV)

        使用烏斯特帶材乾燥機偵測並評估線材厚度的微小波動。品質差的半深色錦綸6長絲織造後織物表面容易出現隱性、橫紋,染色後有明顯的色差缺陷。是高档面料的关键控制指标。

二、加工適應指標(影響織造、彈性、染色)

1.含油量

       GB/T6504 method testing. The content of spinning oil on the surface of the silk directly affects the smoothness of rewinding. Low oil content, high friction of the fiber bundle, easy static electricity and wire breakage; If the oil content is too high, subsequent dyeing will produce oil spots and color spots. Different weaving techniques (warp knitting, machine weaving) need to be matched with corresponding oil content ranges.

2. 恢復

       GB/T6503 testing. Nylon belongs to hygroscopic fibers, and its moisture regain varies with environmental temperature and humidity. Excessive moisture regain can cause the silk cake to adhere and mold easily; Low moisture regain, increased static electricity, and increased weaving breakage. Both warehouse storage and incoming material inspection need to monitor this.

3.網路節點(網路點數)

       Network silk is used to detect the number and uniformity of network nodes. Insufficient network points make it easy for fiber bundles to diverge, increasing the difficulty of weaving; Too many network points cause the silk to harden, affecting the texture of the fabric.

4.染色均勻度

       FZ/T50008 standard is a key testing item for semi dark filament nylon 6. The uniformity of semi extinction TiO ₂ addition directly affects the dyeing effect. Uneven dyeing can result in color spots and variations in the fabric. For ready to wear fabrics and stretch fabrics, this indicator directly determines the yield rate.

三、半消光專屬指標:二氧化鈦(TiO 2)含量

       Semi dark nylon 6 achieves a matte effect by adding titanium dioxide matting agent, which is different from glossy and fully matte silk. Detect TiO ₂ content according to FZ/T 50027. The TiO ₂ content is unstable, and the luster of different silk cakes in the same order may vary in depth, resulting in light and dark stripes on the fabric. This is a key inspection item unique to semi dark filament, and many purchasing customers overlook this indicator, resulting in inconsistent gloss of the finished product.

四、外觀及捲筒檢驗(每管目視取樣)

        依據GB/T16603-2025錦綸彈力絲標準,在標準光源下檢查紗餅外觀:

        髮絲、斷頭、僵硬髮絲、漿塊、油漬、鏽斑

        絲餅成型:端面不平整、塌邊、脫離、蜘蛛網絲

        管材損壞、標籤資訊完整性

        外觀缺陷可直接造成後捲繞過程中的斷頭與布疵。檢驗採取抽樣計劃,依AQL標準判定合格批次。

5.可選定制檢測項目(依客戶需求)

        1.摩擦係數:評估鋼絲與導線之間的摩擦力,預測編織斷頭風險

        2、耐曬、耐老化測試:戶外布料、帳篷、遮陽布料的需求

        3、色牢度測試:皂洗、摩擦色牢度(絲綢製品)

        4、重金屬及有害物質檢測:OEKO-TEX配套檢測,用於貼身服裝、母嬰布料

        5、單絲分離及橫切面形貌檢查:特殊超細旦產品

六、檢驗流程概述

        生產取樣→恆溫恆濕實驗室濕度平衡→儀器性能檢測→外觀及燈光檢查→資料比對說明書→等級判定(優等/一等/合格)→出具質檢報告並隨貨提供批次檢測記錄。

七、為什麼要注意半消光長絲錦綸6的來料檢驗?

       Many textile factories encounter problems such as uneven fabric patterns, unstable shrinkage rates, and a large number of broken ends in warp knitting, which are caused by incomplete testing of the long fibers entering the factory. In addition to conventional strength and shrinkage indicators, the uniformity of TiO ₂ matting agent is a unique risk point for semi dark nylon 6. Early detection reduces losses in subsequent processes and stabilizes fabric quality.